Every deck — wood or composite, $12,000 or $90,000 — is the same five decisions made in the same order. Skipping ahead is how decks fail: surface boards chosen before footing depth is known, railings treated as decoration, flashing treated as optional. This page is the map; each stage has its own chapter.

Stage 1 — Footings: the decision the weather grades

Frost heave lifts any footing whose base sits above the frost line; expansive clay pushes sideways; soft fill settles. The fixes are depth, bearing on undisturbed soil, and a flared or belled base. Helical piers replace depth with torque where digging is impractical. Full chapter: footings & foundations.

Footing section drawingCross-section showing a sonotube concrete footing extending below the frost line, a post base bracket, and a 6 by 6 post rising to the beam. Ground lineFrost line — footing base sits below it 6×6 post, post base bracketFlared footing base
Plate F-1 — Footing section. The base, not the tube, does the work: it must sit below local frost depth on undisturbed soil.

Stage 2 — Frame: the decision the house grades

The ledger board ties the deck to the house, and its flashing is the single detail most responsible for catastrophic deck failure — water trapped behind an unflashed ledger rots the house rim joist silently for years. Joist span tables, beam sizing, lateral-load connectors and corrosion-matched hardware live here. Full chapter: framing & ledger flashing.

Stage 3 — Surface: the decision your feet grade

Composite does not rot, but it gets hot, fades unevenly in its first seasons, and moves lengthwise with temperature. Wood is cooler and cheaper, and asks for stain on a calendar. Hardwood is dense enough to need pre-drilling for every fastener. There is no best material — there is a best match for exposure, budget and how honestly you will maintain it. Full chapter: materials compared.

Deck board profilesCross-section profiles of four deck boards: solid wood, grooved composite, capped polymer, and tropical hardwood, showing thickness and edge differences. Wood, solidComposite, groovedCapped polymerHardwood Actual thickness: a nominal 5/4 board measures about 1 in.; a 2× board about 1.5 in. Stiffness follows thickness.
Plate M-1 — Board profiles. Grooves are for hidden clips, not decoration; solid-edge boards are still required at picture-frame borders and stair treads.

Stage 4 — Rail & stair: the decision the code grades

Guards at 36 inches minimum (IRC, decks more than 30 inches above grade), balusters that reject a 4-inch sphere, stair risers no taller than 7¾ inches with treads at least 10 inches deep. These numbers are not style guidance. Full chapter: railings & stairs.

Stage 5 — Finish & keep: the decision time grades

Pergolas and shade, skirting and drainage, and then the unglamorous calendar — wash, inspect, re-seal, tighten — that doubles or halves the structure's life. Full chapters: pergolas & shade and maintenance & lifespan.

How to use the map. Planning a new deck? Read the stages in order, then run the estimator. Diagnosing an old one? Find the stage whose symptom matches, and read only that chapter. Quoting a builder? Ask which stage each line of their quote belongs to — a quote that cannot be staged is a quote that cannot be checked.